I have a RED 1990 gmc k1500 and the hood and roof are especially bad the sides are no hell either. I have mirror glaze #4, #2 and #26. My question is I don't have a good knowledge about where to start. I know that i need a rotary buffer but what pads do you use for the differant #'s. All I have is an orbital so I am looking for a rotary is there that much of a differance? Do I need #9 after or is #26 ok right after the 2 and 4. I thought that 4 would be needed on the hood and roof and 2 would be aggressive enough on the sides. Am I on the right track? Help is appreciated.